, ʻO Incoloy800H / UNSN08810 / Alloy800H Seamless Tube maikaʻi loa no ka mea hoʻololi wela, ka mea hana pepa a me ka mea hoʻolako |ʻO Guojin

Incoloy800H/ UNSN08810/ Alloy800H Tube Seamless no ka mea hoʻololi wela, mea hana pepa

ʻO ka wehewehe pōkole:

Papa like:
UNS N08810
DIN W. Nr.1.4958


Huahana Huahana

Huahana Huahana

Nā Huahana Loaʻa

Paipu maʻemaʻe ʻole, Pāpaʻa, ʻOkoʻo, Paʻa, Paʻa, Paipu Paipu

Nā Kūlana Hana Hana

Huahana ASTM
Bar B 408
Papa, Pepa a me ka Strip A 240, A 480, B 409, B 906
ʻO nā paipu a me nā mea pono ʻole B 407, B 829
Paipu welo B 514, B 775
ʻO nā mea i hoʻopili ʻia B 515, B 751
Hoʻohui solder B 366
Ke kalaiwa ana B 564

Hoʻohui Kimia

%

Fe

Ni

Cr

C

Mn

Si

S

Cu

Al

Ti

P

Al+Ti

Min

39.5

30.0

19.0

0.06

0.15

0.15

0.85

Max

35.0

23.0

0.10

1.50

1.00

0.015

0.75

0.60

0.60

0.045

1.20

Na Waiwai Kino

ʻO ka mānoanoa 7.94 g/cm3
hehee 1357-1385 ℃

Nā Pono Mechanical liʻiliʻi o Incoloy 800H Alloy ma ka wela lumi

Alloy

Rm N/mm2

RP0.2N/mm2

A5 %

800

500

210

35

800H

450

180

35

ʻO ke kūpaʻa ʻino o Incoloy 800H

Kū'ē ka Incoloy 800H i nā media corrosive.ʻO kāna ʻike nickel kiʻekiʻe e hiki ai ke kū i ke koʻikoʻi i ka haki ʻana o ka corrosion i loko o nā kūlana corrosion aqueous.Hāʻawi ka maʻiʻo chromium kiʻekiʻe i ke kūpaʻa maikaʻi i ka pitting a me ka crevice corrosion crack.He maikaʻi ke kūpaʻa ʻana o ka huila i ka waikawa nitric a me nā ʻakika organik, akā ua kaupalena ʻia ke kūpaʻa corrosion i ka sulfuric acid a me ka waika hydrochloric.ʻO ka pale ʻana i ka corrosion maikaʻi i nā paʻakai oxidizing a me nā paʻakai non-oxidizing, me ka hiki ke hoʻopaʻa i ka corrosion i loko o nā halides.Loaʻa iā ia ke kūpaʻa corrosion maikaʻi i ka wai, ka mahu a me nā hui ʻana o ka mahu, ka ea a me ke kalapona kalapona.

Loaʻa iā Incoloy 800H nā waiwai ma hope

1. ʻOi aku ka maikaʻi o ka corrosion kūʻē i ke kiʻekiʻe kiʻekiʻe aqueous media a hiki i 500 ° C
2. Ke kū'ē maikaʻi i ka corrosion stress
3. Hiki ke hana maikaʻi

Nā wahi noi ʻo Incoloy 800H

1. Nitric acid condenser - kū'ē i ka nitric acid corrosion
2. Paipu hoʻomehana mahu - maikaʻi nā waiwai mechanical
3. Pupu mea hoʻomehana - maikaʻi nā waiwai mechanical
No nā noi a hiki i ka 500 ° C, hāʻawi ʻia ka alloy ma ke kūlana annealed.